Material : SS316L Size : 20 mm Tolerance : ±0.05 mm Weight : 5.0 g
Advantage: Cost reduction by changing manufacturing method from machining to MIM.
Remark: In the de-binding stage of MIM process, the SP mould melts away with the temperature in the furnace, leaving only the metal component with hollow structure inside. This is a very effective method to create such hollow structure inside a metal component.